Zirconium Rod UNS R60705 Round Rod
$19001-49 Ton
$150050-99 Ton
$1200≥100Ton
Payment Type: | L/C,T/T |
Incoterm: | FOB,CFR,CIF,EXW,FCA |
Transportation: | Ocean,Land |
Port: | Tianjin,Shanghai,Ningbo |
$19001-49 Ton
$150050-99 Ton
$1200≥100Ton
Payment Type: | L/C,T/T |
Incoterm: | FOB,CFR,CIF,EXW,FCA |
Transportation: | Ocean,Land |
Port: | Tianjin,Shanghai,Ningbo |
Model No.: Zirconium Alloy
Brand: GNEE
Place Of Origin: China
Shape: Round Bar
Alloy: Alloy
Certification: ISO, RoHS, IBR, AISI, ASTM, GB, EN, DIN, JIS
MOQ: 1ton
Technology: Cold Rolling Hot Rolling
Specification: Zirconium and zirconium alloy rods
Selling Units | : | Ton |
Package Type | : | Standard airworthy packaging |
Picture Example | : |
Zirconium Rod UNS R60705 Round Rod
UNS R60705 zirconium has low thermal neutron absorption cross-section, high strength and hardness, excellent corrosion resistance and ductility. It is widely used in the fields of atomic energy industry, aerospace and biomedicine. It is an important strategic material, also known as As "the number one metal of the atomic age". In order to further increase the stability of zirconium alloy use and reduce processing and manufacturing difficulties, it is essential to connect zirconium alloy materials. Therefore, it is crucial to study the structure and properties of zirconium alloy connections after they are formed through welding technology, and diffusion welding is used as A common material joining method that can be used for welding zirconium and Zirconium Alloys.
We can provide: Zirconium Alloys, Titanium Alloys, Niobium Alloy and other products.
Chemical Properties of Zirconium Alloy 705 Round Bars:
Grade | Zr+Hf | Hf | Fe+Cr | Sn | H | N | C | O | Nb |
R60702 | 99.2% | <4.5% | <0.20% | - | <0.005% | <0.015% | <0.030% | <0.15% | - |
R60704 | 97.5% | <4.5% | 0.2-0.4% | 1.0-2.0% | <0.005% | <0.015% | <0.030% | <0.16% | - |
R60705 | 95.5% | <4.5% | <0.2% | - | <0.005% | <0.015% | <0.050% | <0.16% | 2.0-3.0% |
Mechanical chart of R60705 Zirconium Alloy Welding Rod:
Molecular Weight | 91.22 |
---|---|
Appearance | White |
Melting Point | 1852 °C |
Boiling Point | 3580 °C |
Density | 6506 kg/m3 |
Solubility in H2O | N/A |
Electrical Resistivity | 40.0 microhm-cm @ 20 oC °C |
Electronegativity | 1.4 Paulings |
Heat of Fusion | 5.50 Cal/gm mole |
Heat of Vaporization | 120 K-Cal/gm atom at 4377 °C |
Poisson's Ratio | 0.34 |
Specific Heat | 0.0671 Cal/g/K @ 25 oC °C |
Tensile Strength | 230 MPa |
Thermal Conductivity | 0.227 W/cm/K @ 298.2 K |
Thermal Expansion | (25 °C) 5.7 µm·m-1·K-1 |
Vickers Hardness | 903 MPa |
Young's Modulus | 88 GPa |
R60705 Zirconium Alloy Round Bar Stock Product Image:
Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.
Fill in more information so that we can get in touch with you faster
Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.